Still working on prepping my figure, but I think I'm pretty set on doing the Alucard GK, and I'll probably use Seras as a testing piece to strip later if I don't like it. Won't be able to post again until prolly around the 7th-9th, so we'll see how it goes.
On the subjects of GK's, how careful should I be about using boiling water to heat and bend the e2046 resin? I've been trying to get the duster coat to a position where I can just slip the entire thing on, and paint it as one piece, but I worry the more I heat it the weaker it will get. Could probably paint it in two pieces, but covering the seems on it looks to be a pain.